Chemical Composition
Composition in % (Max)
AM50A
Mg
Remainder
Al
4.5-5.3
Mn
0.28-0.50
Zn
0.2
Si
0.05
Cu
0.008
Ni
0.001
Fe
0.004
Other elements each
0.01
Key Benefits
- Produced in accordance with the strictest quality control guidelines
- Lowest CO2 emitting magnesium production process
- Secure raw material source to support global demand
- A geographic location that offers competitive logistic advantages through proximity to ports and customers
8 Kg Ingot Dimensions
Weight
8kg / 17.6lb
Length
627mm / 24.7ln
Width
128mm / 5ln
Height
67mm / 2.6 in
Typical Physical Properties
Properties
AM50A
Density at 20°C [g/cm3 ]
1.77
Lin.thermal exp.
Coeff [μm/m.K] at
26.0
20-100•c
Thermal conductivity
65
[W/K m] at 20’C
Electrical conductivity
9.1
at 20’C[W/K.m)
Specific heat [kJ/kg K]
1.02
at 20’C
latent heat of fusion
370
[kJ/kg]
Non-equilibrium
620-434
Solidification range[°c]